High content material aluminum alloys, on occasion called EC (electrically
conduction) at times, both comprise no less than 99.5% and are extra electrically conductive
than other a thousand series aluminum. Those are favored alloys in the transformer and switch
gear markets, as they provide the most cost-efficient conductive alloy within the one thousand
series. Despite the fact that other aluminum items have higher aluminum content, maximum
discover those alloys as difficult to source and are exponentially more highly-priced than the
1350 and 1050 alloys.
Those two objects do have one particular difference in where the chemical composition of 1050
has a max has a slightly better max on its silicon content than 1350. It's a completely small
distinction and they're each gift as most values, but there may be a completely small
distinction that could affect critical programs.
Standard Specs: QQA-1876, ASTM B479
Technical Data Sheet
| Chemical Composition Limits |
| Weight% |
Si |
Fe |
Cu |
Mn |
Mg |
Cr |
Zn |
B |
Ga |
V+T |
Cr+Mn+Ti+V |
Others |
| 1350 |
0.1 |
0.40 |
0.05 |
0.01 |
- |
0.01 |
0.05 |
0.05 |
0.03 |
0.02 |
- |
0.03 (each)
0.10 (total) |
1350A
Germany |
0.25 |
0.40 |
0.02 |
- |
0.05 |
- |
0.05 |
- |
- |
- |
0.03 |
0.03 (each) |
Typical Mechanical Properties
| Material |
Temper |
Tensile Strength (N/mm²) |
Elongation in 50mm |
| 1350 Bar |
M |
60 min |
23 |
| 1350 Bar |
H2 |
85 (min) |
13 |